If your purchase order says only "bright polished Titanium Plate", you have not ordered a surface. You have ordered an argument. Four words define neither roughness, nor which faces are treated, nor polishing direction, nor the tolerance that applies after material is removed. Two suppliers can both comply with those four words and ship visibly different plates, and neither can be rejected on paper. A purchasable surface needs six fields: finish method, maximum Ra, which faces, direction or pattern, a visual reference, and the final dimensional tolerance measured after finishing. Get all six in writing or accept that the mill default will decide for you.
This article is about specifying and accepting a surface, not about cleaning a contaminated one. If your problem is free iron, weld heat tint or proving a surface is clean, that is a different job with different tests — see the free-iron contamination and B600 verification guide on this site. Here the question is narrower and more expensive: how do you buy the finish you actually meant?
| Finish | What it actually is | What to write in the PO | Main trap |
|---|---|---|---|
| Pickled | Chemical removal of oxide scale; matte, uniform, not smooth | Pickled per [spec]; Ra not normally specified; faces: both | Assuming pickled means polished or reflective |
| Bright annealed | Vacuum / inert anneal with no oxide; mill-rolled brightness | Bright annealed + retained from mill + which side is visible | Expecting mirror flatness from a coil-rolled bright surface |
| Polished / ground | Mechanical smoothing to a defined roughness | Max Ra (µm), faces, direction, visual sample, defects | No Ra value — nothing to measure or reject |
| Sandblasted | Controlled matte texture from abrasive media | Media type, profile / Ra, faces, cleaning after blasting | Shared carbon-steel media embedding Fe in titanium |
Suppliers list these words side by side as if they were grades of the same thing. They are not. Pickling is a chemical step: acid removes the high-temperature oxide scale from hot rolling or welding and leaves a clean, matte, silver-grey surface. It does not make the surface smooth or reflective. Bright annealing is a thermal step: rolling and annealing under vacuum or inert gas prevents oxide from forming in the first place, so the mill brightness is retained. It is a rolled finish, not a ground one. Polishing or grinding is a mechanical step: abrasive removes metal to reach a defined roughness, and it is the only one of the three where an Ra number is the natural control.
That distinction decides what you can put on the PO. "Pickled" tells the supplier to remove scale; it does not tell them to hit Ra 0.8. "Bright" tells them to preserve a rolled appearance; it does not promise flatness. "Polished" is meaningless until you name a maximum Ra and which faces it applies to. Confusing the three is the single most common reason a buyer receives a technically compliant plate that looks nothing like the sample that won the order.
A published buyer-mistake list from a surface supplier reads like a checklist of what goes wrong in real RFQs: writing only "polished surface"; confusing pickling with polishing; specifying blasting without naming the abrasive; ignoring that grinding and pickling remove material; and relying on photographs alone. Every one of those is a PO problem, not a manufacturing problem.
The reason is simple. A visual phrase without a number cannot be accepted or rejected. If your incoming inspector holds up the plate and says "this is not shiny enough", the supplier can answer "it is bright annealed as ordered" and the dispute has no referee. Put an Ra limit and a visual reference in the PO and the same disagreement becomes a measurement.
Verification action: before you release a surface order, make the supplier state the maximum Ra in micrometres, identify the faces, and confirm whether the number is measured before or after final cleaning. A supplier who cannot name an instrument and a measurement direction has not sold you a controlled finish.
Copy this list into your RFQ. It is short enough to use on a single line item and specific enough to settle a dispute six months later.
Item 6 is the one procurement teams forget most often, and it is where the money is. Grinding, polishing and pickling all remove a small amount of metal. On a 2 mm sheet with a tight tolerance, a finishing pass can consume a meaningful part of the allowable band. If the thickness was measured before finishing, the delivered part can be out of tolerance while the certificate says it passed.
This is the most damaging misconception in surface buying. EN 10204 3.1 mill certificates confirm the base material: heat number, chemistry, mechanical properties and the tests the mill actually ran. They do not certify roughness, polishing direction, cleaning quality or appearance. A flawless 3.1 certificate and a wrong surface can travel in the same box, quite legally.
Surface condition is normally confirmed by separate documents: a roughness report, a visual inspection record, a dimensional report measured after finishing, and — where the part has been handled — a cleaning or free-iron record. Ask for those to be tied to the same heat number and PO line, not issued as free-floating PDFs. The heat-number traceability and PMI guide explains why a document without that link cannot be connected to the material in front of you.
Verification action: ask the supplier which document certifies surface roughness and require it to name the same heat and PO line as the MTC. If the answer is only "the MTC covers it", you have found a supplier who does not separate base material from finish.
Ra is the arithmetic average roughness over a sampling length. That definition matters more than most buyers realise, because two surfaces with the same Ra can look and behave differently. Ra averages peaks and valleys; it does not tell you the deepest valley, the spacing of the grinding marks, or whether a few deep scratches are hiding under an acceptable average. A surface can pass Ra 0.8 and still hold contamination in a narrow groove.
This is why a PO that says only "max Ra 0.8 µm" is better than "polished" but still incomplete. Name the measurement standard and the sampling conditions — the ISO 4287 parameter definition and the ISO 4288 measurement procedure are widely used — and state the direction in which the trace is taken. A longitudinal trace and a transverse trace across the same grinding marks return different numbers. If you care about cleaning, sealing or coating adhesion, agree whether a peak parameter or a visual defect limit belongs in the acceptance criteria as well.
Verification action: ask the supplier to state the instrument, the trace direction and the sampling length used for the reported Ra, and to report it on the same heat and PO line. A number without a method is a number you cannot reproduce in a dispute.
One more distinction saves arguments: brightness is not roughness. A bright annealed sheet reflects light because it has no scale, not because it has been ground flat. A polished sheet can be less reflective than a bright one if the polishing direction scatters light. Buyers who specify by photograph usually end up comparing shine, then measuring a number that was never agreed. Keep appearance and roughness as two separate lines on the PO.
Bright annealing preserves the surface produced by rolling. The sheet leaves the mill with its rolling texture, directional marks and residual stress intact, only without an oxide scale. None of the flatness or forming behaviour of a ground surface should be assumed from the word "bright". On deep drawing or high-speed stamping, a bright sheet can show orange peel or directional streaking if the grain size or rolling direction is wrong for the part, and no amount of polish in the description will change that.
If your component is formed after receipt, state the rolling direction on the drawing and confirm with the supplier which face was the last rolled face. For a stamped gasket or a battery blank this matters more than a marginal Ra improvement. The bright-surface coil and strip options page lists the mill conditions; this article is about making sure the condition you ordered is the condition your forming process actually needs.
Where a part must both form and meet a roughness limit, sequence the operations explicitly: form first, then grind or polish to the agreed Ra, then measure the final thickness. Grinding a flat sheet before forming and expecting the finish to survive the die is a common and expensive misunderstanding.
Finish is not cosmetic. It changes how quickly a surface holds a passive film, how easy it is to clean, and what happens at a weld. The following are the conditions where a correct material specification with the wrong finish still gives you a problem.
A matte pickled surface holds deposits and crevice geometry differently from a smooth polished one. In hot chloride service, a tight gap under scale or a gasket can block oxygen and start local attack. The finish does not change the grade: Grade 2 in a hot crevice is still Grade 2. Where the geometry cannot be designed out, discuss a crevice-resistant grade with the supplier rather than trying to solve the problem with polish alone.
No surface finish survives welding untouched. Heat tint and the oxygen-enriched layer beneath it must be removed before the part returns to corrosive service, and a bright-annealed plate does not exempt you. If the component is welded after finishing, specify the post-weld cleaning and verification in the same PO; otherwise the finish you paid for exists only on the unwelded areas.
Sandblasting with media previously used on carbon steel drives iron into the titanium surface. On a plated or painted part that may be invisible; in a chloride service it becomes a pit initiation site. Name the abrasive and require dedicated media and tools for titanium. The free-iron and pickling guide covers the ferroxyl and copper-sulfate checks used to detect contamination after blasting and grinding.
Abrasive work removes metal. Deep scratches or heavy rolling marks may need extra grinding to reach a mirror finish, and that extra grinding can push a thin sheet below its minimum thickness. Before you demand a mirror surface on a 0.5 mm sheet, agree the minimum delivered thickness with the supplier and confirm how it will be measured after polishing.
A vessel shell may need a pickled interior and a brighter exterior; a stamping blank may need one protected face and one as-rolled face. Writing one finish word for the whole order either over-specifies and wastes money or under-specifies the face that matters. Name faces explicitly.
A photo records light, camera and angle, not Ra. It is useful as a retained visual reference only when the PO also states the numeric roughness and the measurement method. Photographs alone are the classic source of "it looked like the sample" disputes.
Degreasing, pickling and passivation remove contamination and restore the oxide film; they do not create a polished finish. If the requirement is a clean surface for bonding, coating or medical use, write the cleanliness test and acceptance criterion. If the requirement is appearance or roughness, write Ra. Combining the two into one line item is how both get missed.
A surface that is perfect on receipt can be ruined by the next operation: forming, welding, machining, or storage against carbon-steel racks. Agree who owns the surface after delivery and what protection is expected in transit and in the shop. Our stock and cut-to-size service keeps finish requirements on the cut list so they survive slitting and packing.
Choose by what the part must do, not by which surface looks most expensive.
A finish that is justified in one service is wasted money in another. Specifying a mirror polish on a buried tank shell adds cost without changing corrosion performance; specifying a bare pickled surface on a part that must be swabbed clean in a regulated process creates a cleaning problem you will pay for later.
Two surface quotes cannot be compared until they describe the same operation. Normalize them by asking four questions in the same wording: what is the maximum Ra and on which faces; is the price before or after final cleaning; what document certifies the surface; and what is the minimum delivered thickness after material removal. A lower price that omits the polishing step or measures tolerance before finishing is not a lower price.
Ask for the cut-to-size capability and the receiving-weight checks in the same conversation if the finish is applied before cutting: cutting changes which faces are exposed and can change how a plate is weighed and accepted.
A practical way to force an honest comparison is to ask every bidder to fill the same four cells: maximum Ra and faces; measurement method; post-finish minimum thickness; and the document that certifies the surface. When one quote leaves a cell blank, the gap is usually where the cost was taken out. A supplier who says "we will match the sample" without a retained sample reference has not priced a controlled finish at all.
The same discipline applies to quantity breaks. Polishing setup and retained-sample preparation have a fixed cost, so a one-piece polished coupon and a hundred-piece production run quote very differently. Ask for the setup charge as a separate line, and ask whether subsequent repeat orders reuse the same sample and inspection record. This is the point where a low first quote often becomes a more expensive second one.
Example: "Grade 2 plate to ASTM B265, 3.0 mm x 1000 mm x 2000 mm; both large faces pickled; no polishing unless specified; delivered thickness tolerance applies after pickling; surface reported on a roughness/visual record tied to heat number and PO line; EN 10204 3.1 for base material." For a polished part, replace the pickled clause with: "face A ground to max Ra 0.8 µm, longitudinal direction, retained visual sample ref [X], max allowable defects per sample, final thickness measured after grinding."
This is the same discipline used elsewhere on the site: material selection starts with the service, filler classification starts with the procedure, and a surface starts with the measurable requirement. None of them starts with an adjective.
If you remember one sentence from this article, make it this one: the grade is on the certificate, the finish is on the PO, and neither one substitutes for the other. A buyer who writes both down gets a surface that can be accepted or rejected. A buyer who writes only an adjective gets a surface that can only be argued about.
No. Pickling is a chemical step that removes oxide scale and leaves a matte, uniform surface. Polishing is a mechanical step that removes metal to reach a defined roughness. A pickled plate is not automatically smooth or reflective.
No. A 3.1 certificate confirms base material: heat number, chemistry and mechanical properties. Roughness and appearance are normally confirmed by separate roughness, visual and dimensional reports tied to the same heat number and PO line.
Write the method, maximum Ra in micrometres, which faces, the polishing direction or pattern, a retained visual reference, and the final dimensional tolerance measured after finishing. Four adjective words alone give the supplier no acceptance criterion.
Yes. Grinding, polishing and pickling all remove a small amount of metal. On thin or tolerance-critical sheet, state that the delivered thickness tolerance applies after finishing and agree the minimum delivered thickness before ordering.
No. Media previously used on carbon steel can embed iron in the titanium surface and create pit initiation sites in chloride service. Name the abrasive and require dedicated media and tools for titanium, with a cleaning check afterwards.
Finish alone does not solve hot chloride crevice corrosion. A smooth surface is easier to keep clean, but grade and joint design govern. If the geometry creates a tight hot crevice, discuss a crevice-resistant grade rather than relying on polish.
Yes if the faces have different jobs. A vessel shell may need a pickled interior and a brighter exterior; a stamping blank may need one protected face. Writing one finish word for an entire order usually over-specifies some faces and under-specifies the one that matters.
Need a finish written into the PO, not left to the mill default?
Send the grade, product form, dimensions, which faces matter, the service medium and any Ra or visual requirement. We will quote the finish route and the inspection documents together, and tell you where a requested finish is unnecessary cost. Send your RFQ on WhatsApp: +86 188 2967 9311 — or use the online inquiry form.
Контактное лицо: Wang Xiaoning
Телефон: +86-917-355-7966
Эл. почта: [email protected]
WhatsApp: +86 188 2967 9311
Компания: Shaanxi Qianyi Tuoda Technology Co., Ltd
Адрес: Floor 4, Building 4, No. 188 Gaoxin Avenue, High-tech Zone, Baoji City, Shaanxi Province, China