| Specification | Alloy family / Pure Ni N200 N201, Ni-Cu Monel 400 K-500, Ni-Cr-Fe Inconel 600 625, Ni-Cr-Mo C276 C22, Ni-Fe-Cr Incoloy 800 825 |
|---|---|
| Applicable Standard | Applicable ASTM / B160 B161 B162, B164 B165 B127, B166 B446 B444, B574 B575 B622, B408 B407 B423; ASME SB editions |
| Material Condition | Filler classification / AWS A5.14 ASME SFA-5.14 ERNi-1 ERNiCu-7 ERNiCr-3 ERNiCrMo-3 ERNiCrMo-4 ERNiCrMo-10 |
| Inspection & Packaging | Fabrication route / groove cleaning, interpass cap, PWHT or solution anneal, work-hardening forming allowance, corrosion re-test, per-family WPS |
Product Description: One nickel alloy order can hide five families, each with its own groove, filler, interpass, PWHT, forming and re-test rules. Build a family matrix PO.
One nickel alloy purchase order can contain five alloy families, and those five need five different sets of welding rules: groove cleaning, filler, interpass temperature, PWHT, forming and re-test differ across pure nickel, Ni-Cu, Ni-Cr-Fe, Ni-Cr-Mo and Ni-Fe-Cr stock. Our Ni200 versus Ni201 guide, nickel products by medium, Monel 400 pump valve page, nickel-steel clad plate page, Monel versus Inconel guide, C276 versus C22 guide, K-500 versus 400 guide and alloy family guide settle grade selection and which standard to order. These pages decide which alloy to buy. This one starts after that decision: how the chosen family is fabricated, welded and released. There are eight rejection triggers and one 14-line matrix PO.
We do not rebuild grade comparison tables or repeat the corrosion conclusions those pages already cover. This is the fabrication and welding evidence layer: a matrix that turns a chosen family into a qualified method statement, a filler lot, a temperature log and a signed release. A certificate says what the metal is; a method statement says what was done to it. Where a number depends on an edition, we give the verification action instead of one false figure.
Read the first three rows before the first bevel is cut; they fix the family split, the WPS rule and the filler rule. The rest become shop-floor checks an inspector signs per family.
| Item | What the fabrication decision turns on |
|---|---|
| The short answer | One order can hold five nickel alloy families, each with its own groove, filler, interpass, PWHT, forming and re-test rules |
| The core hook | One qualified WPS cannot be reused across two families; qualification is family, filler and condition specific |
| The filler trap | Matching filler does not mean the same base-metal grade; AWS A5.14 is separate from a B160 or B162 product spec |
| Five product-spec groups | B160 B161 B162, B164 B165 B127, B166 B446 B444, B574 B575 B622, B408 B407 B423 |
| The public conflict | Interpass caps and sensitization windows disagree across datasheets and codes; no single value, six verification actions |
| Six verification actions | Name the edition, the state, the method, the map, the reviewer and the file |
| The release document | A 14-line Alloy-Family Fabrication Matrix PO, per family, with basis, criterion and sign-off |
| The one decision | Who signs each family line before a weld is released, and which document governs a conflict |
Row three hides most rework. Our nickel products range shows the forms one order can carry and our EN 10204 3.1 certificate page shows a traceable record. Neither tells a welder which filler class or interpass cap applies. A stockholder can certify grade, dimension and heat number; it cannot qualify a WPS for five families at once.
The phrase nickel alloy on a purchase order is a category, not a welding instruction. One order can list N201 tube, Monel 400 plate, Inconel 625 bar, C276 pipe and Incoloy 825 tube. A buyer sees five line items under one heading; a shop must see five weld procedures. If it writes one WPS and stamps every joint with it, four lines are welded outside their qualified range.
The families are separated by chemistry and by the standards governing their product forms. Our B160 B164 B574 B446 bar specification page shows one order can cover several bar standards, our N6 Ni201 Monel 400 page shows grades in different families, and our alloy family guide is where the split begins. Those pages answer which alloy to buy; the fabrication question is what each family demands in the shop.
One purchase order, five alloy families, five WPS documents. A certificate says what the metal is; a method statement says what you did to it.
A WPS proven on one family does not describe a joint in another.
A WPS is qualified against a base-metal grouping, a filler classification, a process, a position and essential variables. Change the family and you change the metallurgy: pure nickel has almost no alloying reserve, Ni-Cu ages differently from Ni-Cr-Fe, and Ni-Cr-Mo grades are low-carbon and sensitive to heat input and contamination. One PQR cannot cover all five. Our WPS and NDT qualification guide makes the parallel point for another material family.
Two document families are often confused. The ASTM B specifications and their ASME SB counterparts are product specifications; they state what the mill must meet. Our B161 B163 B622 B423 pipe page and B162 B575 plate page are product documents. A WPS is a fabrication document qualified by a PQR. Confusing them is how a buyer believes a mill certificate authorised a weld.
Sensitization is already written up on this site, so we do not present it as new. Our N6 nickel plate sensitized corrosion article covers the mechanism. This article only assigns the process witness: which edition, which corrosion test, which specimen location and who signs the re-test for the family in question.
A product specification gets material to the gate. A qualified WPS governs the arc. They are separate documents.
Filler for nickel alloys is classified under AWS A5.14 and ASME SFA-5.14, a system built around bare electrodes and rods, not the ASTM B product specification of the base metal. ERNi-1 belongs to pure nickel, ERNiCu-7 to Ni-Cu, ERNiCr-3 and ERNiCrMo-3 to Ni-Cr-Fe, ERNiCrMo-4 and ERNiCrMo-10 to Ni-Cr-Mo, and the Ni-Fe-Cr family is served by classes that sources map differently. Our nickel wire classification page shows a wire diameter table is not a filler classification.
Matching is the trap. Filler wire carries deoxidisers such as titanium, aluminium or niobium that the wrought base metal does not, so its chemistry is deliberately different. Incoloy 825 is commonly welded with ERNiCrMo-3, a 625-type wire, not a wire of the N08825 grade. Our C276 selection guide and C276 versus C22 guide sit where ERNiCrMo-4 and ERNiCrMo-10 are named. Matching means fit for the family and service, not the same grade name.
The mapping for 800, 800H and 825 is where sources disagree: some assign ERNiCr-3, some ERNiFeCr-1, and 825 is often given ERNiCrMo-3. We print no winner. Confirm the class against the AWS A5.14 edition and qualified WPS in the PO, and record it with its lot, not the base-metal grade.
A matching filler is a classification chosen for the joint, not a copy of the base-metal grade. Write the AWS A5.14 class and its lot.
Two numbers cause most arguments on a nickel fabrication floor: the maximum interpass temperature and the sensitization or solution-anneal window. Published values disagree by family, code, thickness and datasheet edition. Some give a hard cap, some a range, some say a family needs no preheat while another needs a minimum. One number copied from a supplier table will be wrong for at least one family. Our sensitized corrosion article explains why time at temperature matters; here we decide how to record it.
| Quantity | Where sources disagree | What we print | The action |
|---|---|---|---|
| Maximum interpass temperature | Hard caps, ranges and family limits across codes | No single cap | Name the WPS, alloy, thickness, edition; log each pass |
| Sensitization and solution-anneal window | Different ranges by carbon level and test method | No single window | Name the test, specimen location and edition |
| Preheat requirement | Some families welded cold, others given a minimum | No single prescription | Resolve from the qualified WPS and PO |
| PWHT, age or as-welded decision | Solution anneal, age harden or a waiver conflict | No single cycle | Record the route, furnace chart and sign-off |
| Filler mapping for 800 and 825 | ERNiCr-3, ERNiFeCr-1 and ERNiCrMo-3 each quoted | No single class | Confirm against the A5.14 edition and WPS |
Our B162 B575 plate page and seamless pipe page are product documents that stop at the mill gate, and our nickel plate weight calculator is a commercial tool. None carries the weld variables. Six actions settle the numbers instead of one favourite value.
Six verification actions when the fabrication data disagrees
Name the version, the state, the method, the points, the reviewer and the file. That is cheap at planning and costly after release.
The matrix below is the article in one table. Each cell names a document, a class or a duty rather than a single temperature wrong for half the order. Read it as a PO template, not a datasheet.
| Alloy family and product specs | Groove and cleaning | Filler class (AWS A5.14) | Preheat, interpass, PWHT | Forming and hardening | Re-test and release |
|---|---|---|---|---|---|
| Pure nickel N200 N201 / B160 B161 B162 | Dedicated tools; remove lead, sulphur, phosphorus, oil | ERNi-1 class | Cap per WPS; anneal condition recorded | Ductile; large allowance; intermediate anneal | Corrosion coupon if service demands; MTC heat map |
| Ni-Cu Monel 400 K-500 / B164 B165 B127 | Dedicated tools; copper-bearing soil controlled | ERNiCu-7 class | K-500 age state recorded before and after welding | Aged condition limits cold forming | Hardness and age-state check; per-family WPS |
| Ni-Cr-Fe Inconel 600 625 / B166 B446 B444 | Dedicated stainless tools; no free iron | ERNiCr-3 or ERNiCrMo-3 class | Low heat input; interpass log per pass | Rapid work hardening; constant feed | ASTM G28 or named method; specimen location |
| Ni-Cr-Mo C276 C22 / B574 B575 B622 | Strict segregation; low-carbon cleanliness | ERNiCrMo-4 or ERNiCrMo-10 class | Low heat input; interpass cap per WPS | High work-hardening rate; generous bend allowance | Corrosion re-test with method and edition |
| Ni-Fe-Cr Incoloy 800 825 / B408 B407 B423 | Dedicated tools; no carbon-steel contact | Class confirmed against A5.14 edition; sources conflict | Solution-anneal state recorded | Austenitic work hardening; intermediate anneal | Corrosion coupon; heat map; filler lot traceability |
Our Nickel 200 B161 pipe stock page and pure nickel caustic tube page are the pure nickel end of row one, and our N6 Ni201 Monel 400 page shows two families quoted side by side. Side-by-side quoting on a web page is not side-by-side welding: the six columns must be answered again for every family.
A matrix is useful only if a planner can read one row and know what to write in the WPS. The five short sections name the product specs, filler family and forming behaviour for each family, without reopening the corrosion arguments settled on the linked pages.
Family 1: pure nickel N200 and N201, B160 B161 B162
Commercially pure nickel is soft and almost free of alloying reserve, so its sensitivity is to contamination, not hardening. Groove faces must be cleaned of lead, sulphur, phosphorus and oil with dedicated tools, and ERNi-1 is the named filler family. Our Ni200 versus Ni201 guide settles which grade suits the temperature; our B161 pipe page and caustic tube page cover the forms. This row records the cleaning method, filler lot and anneal condition.
Family 2: Ni-Cu Monel 400 and K-500, B164 B165 B127
Ni-Cu uses ERNiCu-7 and needs the heat-treatment condition in the WPS, because K-500 is age hardened and 400 is not. Our K-500 versus 400 age-hardening guide covers the split and our Monel 400 pump valve page covers where it is bought. This row records whether the part arrived solution annealed or aged, whether welding preceded ageing, and who signed the age-state check.
Family 3: Ni-Cr-Fe Inconel 600 and 625, B166 B446 B444
Ni-Cr-Fe uses ERNiCr-3 or ERNiCrMo-3 and is the row where a sensitization window and corrosion re-test enter the ITP. Low heat input, a per-pass interpass log and a specimen-location map are the witnesses. Our sensitized corrosion article owns the chemistry; this row assigns the test method, edition and signatory. Work hardening is rapid, so reduction and intermediate anneal are recorded per family.
Family 4: Ni-Cr-Mo C276 and C22, B574 B575 B622
Low-carbon Ni-Cr-Mo uses ERNiCrMo-4 for C276 and ERNiCrMo-10 for C22, and demands strict segregation from carbon steel and other families. Our C276 versus C22 guide and C276 selection guide settle which grade to buy. This row records dedicated tooling, low heat input, the interpass cap from the WPS, the PWHT decision and the corrosion re-test with method and edition.
Family 5: Ni-Fe-Cr Incoloy 800 and 825, B408 B407 B423
Ni-Fe-Cr closes the matrix and is the clearest filler conflict: 800 and 825 are quoted with different AWS A5.14 classes, and 825 is often welded with ERNiCrMo-3, not the N08825 grade. Our Monel versus Inconel selection page and alloy family guide show how often cross-family comparisons are made. This row records the chosen class with its edition and lot, the solution-anneal state, and the reviewer who confirmed the mapping.
Nickel alloys work harden ahead of a tool or bend die and hold heat at the worked surface. That changes the forming allowance for every family, but not by the same amount. Pure nickel is ductile, Ni-Cr-Mo and Ni-Cr-Fe harden fast, and an age-hardened K-500 part cannot be cold formed on the assumption used for solution-annealed 400. Our nickel products by medium page shows why one order mixes conditions, and our K-500 age-hardening guide shows condition drives hardness.
We print no bend radius, reduction limit or anneal temperature, because each depends on family, thickness, condition, edition and the qualified method statement. Confirm the condition on the certificate and verify the allowance at the first article with a hardness traverse. Our free-iron and pickling guide explains why a formed surface also needs a documented clean, and our Baoji stock supplier page gives the dispatch context. A part with a hardened skin and no cleaning record is a reject regardless of dimensions.
Residual stress and springback are shop-floor facts
Rough symmetrically, record the sequence and intermediate anneal as ITP hold points, and sign the forming step per family. Cold work is inherited by the next weld.
None of these means a nickel alloy is a poor purchase. Each names what to measure, the basis document, the judgement and the dispute action, applied by family and process rather than once for the order. Our nickel products range and certificate page cover the stock and record side; these triggers are the fabrication evidence side.
Pull the WPS and PQR for every weld and compare the family, filler class and essential variables against the joint. Judge against the qualified range, not the job title. A WPS qualified on pure nickel does not cover a Ni-Cr-Mo joint, which our alloy family guide shows is a separate family. Hold the lot, quarantine out-of-range welds, and require a family-specific WPS.
Read the filler lot certificate against the WPS and check that an ERNi-1, ERNiCu-7 or ERNiCrMo-4 class is named, not the plate designation. Judge against the AWS A5.14 edition in the PO. Our wire selection page shows a wire table is not a classification. Hold the joint, record the lot, and confirm the mapping with an independent reviewer.
Reconstruct the interpass record from the weld log and check for a calibrated pyrometer or crayon reading on each pass. Judge against the WPS, not a datasheet. Our WPS and NDT qualification page makes the parallel point for another family. With no log, hold the weld, review heat input, and require re-qualification or a documented disposition.
Compare the furnace chart and heat-treatment procedure against the family and the edition named in the PO. Judge against the qualified route, not a generic cycle. Our sensitized corrosion article owns the mechanism; the failure is a document mismatch. Hold the lot, identify which edition governed, and require a corrosion coupon with a recorded specimen location.
Inspect the groove and swab for free iron with a recorded kit and expiry, and check the tool segregation log. Judge against the PO cleanliness clause. Our free-iron and pickling guide sets out the chemistry for another reactive family. Quarantine the joint, re-clean to the documented procedure, re-test a control area, and require a signed cleaning record.
Check the certificate and traveller for the age state before and after welding and reconcile them with the WPS. Judge against the PO condition clause. Our K-500 versus 400 guide shows condition drives hardness, and an unqualified re-age is hardness the shop created. Hold the part, take a hardness traverse, and require a qualified age cycle or waiver.
Compare the forming method statement, reduction per pass and anneal record against the family and condition on the certificate. Judge against the approved method statement. Our nickel-steel clad plate page and Monel versus Inconel page are distinct upstream products that cannot share one route. Segregate the parts, measure springback, and re-qualify the allowance.
Open the re-test report and confirm the test standard, edition, specimen location in weld metal, HAZ and base metal, and the acceptance criterion for the family. Judge against the ITP and sign-off column. Our 3.1 certificate page shows the form a traceable record takes. Hold the release, rebuild the coupon with an independent witness, and re-sign per family.
The recurring failure is a one-line PO that says nickel alloy, weld to code. Each line below is answered with a document, criterion and signature; lines three to seven are written per family. Never merge lines eight and nine or leave line fourteen unsigned.
| # | Matrix PO line, by family | Basis document | Acceptance criterion | Sign-off |
|---|---|---|---|---|
| 1 | Family, grade, UNS, governing ASTM B or ASME SB spec per line item | PO and mill test certificate | Family, grade, edition match | Buyer QA and storekeeper |
| 2 | Groove geometry, cleaning, dedicated tool segregation, all families | WPS and weld preparation drawing | No free iron, lead, sulphur, phosphorus, oil | Welding supervisor |
| 3 | Pure nickel N200 N201 (B160 B161 B162): ERNi-1, anneal condition | AWS A5.14 edition, WPS, filler lot certificate | Class and lot match the WPS | Welding engineer |
| 4 | Ni-Cu Monel 400 K-500 (B164 B165 B127): ERNiCu-7, age state | AWS A5.14, PO condition clause, WPS | Filler class and age condition recorded | Welding engineer and buyer QA |
| 5 | Ni-Cr-Fe Inconel 600 625 (B166 B446 B444): ERNiCr-3 or ERNiCrMo-3, interpass cap | AWS A5.14, WPS, PQR | Class and per-pass interpass log inside range | Welding inspector |
| 6 | Ni-Cr-Mo C276 C22 (B574 B575 B622): ERNiCrMo-4 or ERNiCrMo-10, low heat input | AWS A5.14, WPS, heat-input record | Class and heat input recorded per pass | Welding engineer |
| 7 | Ni-Fe-Cr Incoloy 800 825 (B408 B407 B423): filler mapping confirmed from conflicting tables | AWS A5.14 edition, qualified WPS | Chosen class recorded with edition, not assumed | Welding engineer and buyer QA |
| 8 | Preheat and maximum interpass per family, measured per pass | WPS, calibrated pyrometer or crayon record | Readings inside cap, instrument ID logged | Welding inspector |
| 9 | Sensitization window, solution anneal, PWHT or as-welded decision per family | WPS, heat-treatment procedure, furnace chart | Route, cycle, edition recorded or waiver signed | Heat-treatment supervisor and QA |
| 10 | Age-hardening condition of Monel K-500 before and after welding | PO condition clause, qualified age procedure | Age state recorded, no unqualified re-age | Buyer QA |
| 11 | Forming allowance, reduction, springback, intermediate anneal per family | Approved forming method statement | Reduction and anneal recorded, dimensions inside drawing | Forming supervisor |
| 12 | Corrosion re-test coupon per family, method, edition, specimen location | ITP and named corrosion test standard | Location, method, edition, result recorded | Independent laboratory and QA |
| 13 | Filler lot, base-metal heat number, heat-to-weld map after cutting | Filler certificate, MTC, job traveller | Every weld traceable to filler lot and base heat | Storekeeper and inspector |
| 14 | ITP hold points, nonconformance, family-specific final release | This matrix PO and the ITP plan | Every line answered and signed per family | Quality lead and buyer |
Line five is often answered with one note for two families, line seven with a handbook class, line twelve with no specimen location, and line fourteen with no signature. Our bar specification page, plate specification page and seamless pipe page separate product identity from fabrication work; 3.1 certificate page and WPS and NDT qualification page show a witnessed record. nickel products range, N6 Ni201 Monel 400 page and Baoji stock supplier page trace a released weld back to stock.
Choose a per-family fabrication matrix PO if:
Escalate to a quality review or a fabrication dispute if:
Choose a different route or pause the job if:
The whole subject reduces to one sentence: one nickel alloy order can hold five families, and a method statement not written per family has already lost the argument about how the metal is welded and released. When you enquire, send the alloy family and grade, the ASTM B or ASME SB edition, product form and dimensions, delivery condition, drawing, service environment and the 14-line matrix PO. We are a Baoji China Titanium Valley stockholder holding about 30 tonnes of nickel products in stock alongside our titanium ranges. We cut to non-standard and small-batch sizes, work from customer drawings, certify to ASTM, ASME and GB standards, export-pack in house and dispatch confirmed in-stock orders the same day. Send us the alloy schedule and the family matrix, and we will tell you honestly what we can ship from stock and which fabrication decisions belong with your quality team. Request a quote →
Because a welding procedure qualification is tied to a base-metal family, a filler class and a heat-treatment condition. A WPS qualified on pure nickel does not cover a Ni-Cr-Mo joint with a different filler and interpass rule. Each family needs its own WPS and PQR, or a written extension naming the new family. Confirm the range against the WPS and the PO edition.
No. Matching means the filler is chosen for the family and service, classified under AWS A5.14 or ASME SFA-5.14, not that it carries the base-metal grade. Filler wire contains deoxidisers, so its chemistry differs from the plate it joins. Incoloy 825 is commonly welded with ERNiCrMo-3, not a N08825 grade wire. Confirm the class against the WPS.
Pure nickel N200 and N201 use B160 for rod and bar, B161 for pipe and tube, B162 for plate. Ni-Cu Monel uses B164, B165, B127. Ni-Cr-Fe Inconel uses B166, B446, B444. Ni-Cr-Mo C276 and C22 use B574, B575, B622. Ni-Fe-Cr Incoloy 800 and 825 use B408, B407, B423. Confirm the product form and edition in the PO, and use the ASME SB edition when the contract calls for it.
We do not print one. Published caps differ by family, code and datasheet edition, and some sources give a maximum while others give a range. Name the WPS, alloy, thickness and edition, measure each pass with a calibrated pyrometer or crayon, and log the reading with the instrument identity. Resolve the value from the qualified WPS, not a supplier table.
The window depends on family, carbon level, time at temperature and the test method, and datasheets and codes quote different ranges. Some families are solution annealed, some age hardened, some left as welded with a waiver. We give no single cycle. Name the edition, state the specimen condition, fix the corrosion test and location, and record the furnace chart and sign-off.
Fourteen lines, each naming what to check, the basis document, the acceptance criterion and who signs, written per family. They cover the product spec, groove cleaning, filler class, interpass, PWHT, forming allowance, the heat-number map, the corrosion coupon, hold points and final release. A matrix PO without a signature per family is a note, not a release record.
Yes. Radiographic or dye-penetrant acceptance is one line of the record. A cross-family WPS, a filler lot recorded as the base-metal grade, an interpass reading with no log, a sensitization cycle from the wrong edition and a coupon with no specimen location are valid holds on a weld that passed NDT. Judge each trigger against the PO and hold the joint before release.
Tell us your requirement — grade, size and quantity. We reply within 24 hours.
Prefer chat? WhatsApp +86 188 2967 9311 or email [email protected].
Contact Person: Wang Xiaoning
Tel: +86-917-355-7966
Email: [email protected]
WhatsApp: +86 188 2967 9311
Company: Shaanxi Qianyi Tuoda Technology Co., Ltd
Address: Floor 4, Building 4, No. 188 Gaoxin Avenue, High-tech Zone, Baoji City, Shaanxi Province, China