Welcome to Shaanxi Qianyi Tuoda Technology Co., Ltd
EnglishРусский中文
  • Titanium Clad Plate Alternative \| Gr2/Ti-Steel Composite, Stock + Project Supply
Titanium Clad Plate Alternative \| Gr2/Ti-Steel Composite, Stock + Project Supply

Titanium Clad Plate Alternative \| Gr2/Ti-Steel Composite, Stock + Project Supply

Specificationtitanium clad plate alternative stock supplier, titanium steel clad plate ASTM B898, Gr2 titanium clad plate alternative to solid titanium, TA2 ti-steel composite plate, explosion bonded titanium clad

Product Description: Titanium clad plate alternative to solid titanium from Baoji. Gr2/Ti-steel composite per ASTM B898, project supply from ready TA2 stock, UT bonded, MTC traceable, export packed. Quote within 24h.

Request a Quote Contact Sales

Product Overview

Titanium Clad Plate Alternative Stock Supplier | Gr2 Ti-Steel Composite

Meta Description: Titanium clad plate alternative to solid titanium from Baoji. Gr2/Ti-steel composite per ASTM B898, project supply from ready TA2 stock, 100% UT bond check, MTC EN 10204 3.1 traceable, export packed. Quote within 24h.

Overview

When a project specifies solid Gr2 Titanium Plate but the budget or wall-design does not justify full-thickness titanium, a titanium clad plate is the engineering-sound alternative: a thin TA2/Gr2 corrosion layer metallurgically bonded to a carbon-steel or stainless-steel backing. We are a Baoji titanium inventory holder with 800 tons total titanium stock (≈400 tons plate). Our role as a clad-plate alternative supplier is twofold:

  • Stock side: TA2/Gr2 cladding-layer material and thin Titanium Plate held in ready stock, cut to size
  • Project side: ti-steel clad plate supplied via explosion-bonded / explosion+roll route through qualified clad mills, to drawing, with full traceability

This page explains what clad plate is, when it replaces solid titanium, how we qualify it, and how to enquire without ambiguity.

What Is a Titanium Clad Plate

A bimetal composite: corrosion-facing layer = titanium (Gr1/Gr2/Gr7), structural layer = carbon steel (Q345R/A516 Gr.70) or stainless (304/316L). Two manufacturing routes:

Route Bond Method Typical Use
Explosion bonded Explosive welding, metallurgical bond at interface Reactors, shells, large walls
Explosion + hot roll Explosion weld then roll-reduce Uniform thickness, larger coils/plates

Standards referenced: ASTM B898 / ASME SB-898, GB/T 8547 (domestic), with cladding layer per ASTM B265.

Clad Plate vs Solid Titanium — Honest Comparison

Dimension Solid Gr2 plate Ti-steel clad plate
Corrosion face Full titanium Titanium only where medium touches
Structure Titanium carries all load Steel carries load, Ti carries corrosion
Weight Lighter than steel Heavier than solid Ti, lighter than full steel thick wall
Material cost Higher titanium kg Less titanium → lower material cost (project-specific)
Welding Ti-only procedure Requires clad-weld procedure (butter layer / transition)
Lead time Stock gauges fast Project-made, lead time confirmed per spec
Best for Small HX, pure-Ti mandatory parts Large shells, reactor walls, liners

We do not quote a fixed "save 30%/50%" number — savings depend on clad ratio, backing steel grade, and welding procedure. We help you calculate it from the drawing.

Typical Spec We Supply

Item Range
Cladding grade Gr1 / Gr2 / Gr7 (TA1/TA2/TA9)
Cladding thickness 1.0–10mm (custom ratio)
Backing Q345R / Q235B / A516 Gr.70 / 304 / 316L
Backing thickness 3–50mm+
Total thickness 6–120mm (project dependent)
Width × Length Up to 3000×12000mm (mill capability, confirmed per PO)
Bond shear strength ≥120 MPa typical (per ASTM B898 / GB/T 8547)
NDT 100% ultrasonic bond-line scan

Where Clad Plate Replaces Solid Ti

  • Chemical reactor shell & tower walls (chloride / dilute acid)
  • Desalination MSF/MED evaporator shells
  • Pressure vessel liners where code allows clad construction
  • Seawater cooling shells, brine chambers
  • Ash/FGD scrubber walls, chimney liners (with procedure review)
  • Large acid tanks where full solid Ti wall is over-specified

Our Supply Model (No Fake "Always in Stock" Claim)

  • Cladding-layer stock: TA2/Gr2 thin+mid plate (part of 400t plate pool) — real ready stock
  • Clad plate itself: project order, matched to qualified clad mill, lead time quoted honestly
  • Alternative quick route: solid TA2 liner cut from stock + fitted inside steel shell (loose liner) for some non-code applications — faster than waiting on explosion bond
  • We review drawing → propose clad ratio or liner alternative → quote both paths if sensible

Bond Quality & Acceptance

  • 100% UT along bond interface (no delamination acceptance)
  • Shear/peel coupon test per ASTM B898 / GB/T 8547
  • Diffusion-layer control to avoid brittle intermetallic over-growth
  • Cladding-side pickled, steel-side primed/blast as agreed
  • Flatness per order spec (≤3mm/m tight option on request)

Certification & Traceability

  • Cladding layer: EN 10204 3.1 from titanium mill (heat-number traceable)
  • Backing steel: mill 3.1 for base material
  • Clad plate: manufacturer inspection cert referencing both heat numbers + bond test record
  • 3.2 (SGS/BV/TÜV witness) on request at buyer cost
  • Heat number on cladding tag = MTC line = crate tag (no mix)

True 3.1 is issued by the producing mill's independent inspection function — we supply the mill cert, not a trader-signed substitute.

Welding & Fabrication Notes

  • Cladding side: Gr2 filler, argon backing
  • Backing side: matched carbon/stainless WPS
  • Transition joint / butter layer required at clad interface — procedure supplied by fabricator or reviewed together
  • We do not issue WPS/PQR; we supply material + test data for your ASME/PED shop to qualify
  • Cutting: plasma/waterjet on clad plate; avoid carbon-steel-contact on Ti face

Export Packaging

  • Ti face: PE film + kraft interleave
  • Edge guards, foam on corners
  • Fumigated wooden crate / steel-frame skid for heavy clad plates
  • Moisture barrier for long-sea
  • Marking: cladding grade, backing grade, heat Nos., dims, PO ref

Enquiry Template (Copy-Paste)

Project: ___
Medium: ___ (chloride ppm, temp, pH, acid type)
Alternative goal: cost / weight / lead time
Cladding grade: Gr2 / Gr7 / TA2
Clad ratio: e.g. 3mm Ti + 20mm steel
Backing: Q345R / A516-70 / 316L
Total thickness × width × length: ___
Qty: ___ pcs / ___ ton
Standard: ASTM B898 + B265
Cert: EN 10204 3.1 (cladding + backing) / 3.2 if needed
Welding docs: WPS provided by buyer / need material-only
Destination port: ___

FAQ — Titanium Clad Plate Alternative

Q1: Do you keep explosion-clad plates in ready stock?
A: Cladding-layer TA2 is stock; finished clad plates are project-made via qualified mills. For urgent non-code cases we propose a cut-to-size solid TA2 loose liner as a faster alternative.

Q2: Is clad plate acceptable for ASME pressure vessels?
A: Yes, clad construction is covered by ASME rules, but the stamp holder qualifies WPS/PQR. We supply material + traceable certs to support their dossier.

Q3: How do you prove bond quality?
A: 100% UT bond-line scan + shear/peel coupon per ASTM B898 / GB/T 8547. Report ships with plate.

Q4: Can you do loose liner instead of metallurgical clad?
A: For selected services (no cyclic thermal shock, mechanical fix acceptable), yes — faster, from TA2 stock.

Q5: What clad ratio is economical?
A: Common 1.5–3mm Ti on 16–30mm steel, but optimum depends on corrosion allowance + fabrication cost, not a fixed rule.

Q6: Lead time?
A: TA2 liner from stock: same-day cut if confirmed before 3 PM China time. Explosion-clad project: lead time quoted after drawing review (mill schedule dependent).

Q7: Certificate for two metals?
A: Cladding 3.1 + backing 3.1 + clad manufacturer bond-test record. 3.2 witness on request.

Q8: Can you supply Gr7 cladding for reducing acid?
A: Yes, Gr7 (Pd) cladding on request — lead time extended by specialty titanium availability.

Q9: Minimum project size?
A: No hard MOQ on stock TA2 liner; clad-plate project MOQ set by mill, quoted per enquiry.

Q10: How is price built?
A: Titanium layer kg × clad ratio + backing steel + bond process + cutting/cert. We break it down — no bundled mystery number.

Request a Quote

Email: sales@[yourdomain].com

Send drawing/CLAD spec + medium condition. We return: (1) clad route feasibility, (2) solid-Ti-liner alternative, (3) stock availability of cladding layer, (4) honest lead time + EXW/FOB quote within 24 working hours.


About: Baoji Titanium Valley inventory holder. TA2/Gr2 plate ready stock + ti-steel clad plate project supply per ASTM B898. Explosion-bonded / roll-clad route via qualified mills, UT bond-verified, EN 10204 3.1 traceable, export packed. We give the alternative, not just the upsell.

titanium clad plate alternative stock supplier

Get a Free Quote

Tell us your requirement — grade, size and quantity. We reply within 24 hours.

Captcha code

Prefer chat? WhatsApp +86 188 2967 9311 or email sales@sxqytd.com.