Specification1. We maintain ready stock of corrosion resistant nickel alloy tube, covering a wide range of nickel-based alloys for demanding industrial systems where pure nickel and stainless steel cannot meet ser
Reference Price$50.00 – $80.00

Product Description: Corrosion resistant nickel alloy tube stock from Baoji — pure nickel N02200/201, Monel 400, Inconel 600/625, Incoloy 825, Hastelloy C-276. Seamless per ASTM B161/B163/B165/B167/B407/B423/B444/B622, ma

Request a Quote Contact Sales

Product Overview

Corrosion Resistant Nickel Alloy Tube Stock | Grade-by-Medium Selection, Seamless, PMI 3.1

Meta Description: Corrosion resistant nickel alloy tube stock — N02200/201, N04400, N06600/625, N08825, N10276. Seamless per ASTM B161/B163/B165/B167/B407/B423/B444/B622, matched to caustic, seawater, acid and sour service. PMI per heat, EN 10204 3.1, 3.2 TPI PO-fronted.

"Corrosion Resistant" Is Not One Alloy — It's a Match

Nickel alloy tube does not win by being "more expensive". It wins by matching the actual stream:

  • Caustic soda → pure nickel (200/201)
  • Seawater / brine / HF → Monel 400 (N04400)
  • Hot oxidising gas / furnace → Inconel 600/601
  • Chloride + seawater + strength → Inconel 625 (N06625)
  • Sulfuric / phosphoric acid → Incoloy 825 (N08825)
  • Mixed / reducing / wet-chlorine acid → Hastelloy C-276 (N10276)

Quote without medium+temperature = guess. We don't guess.

Grade ↔ Standard ↔ Service Map (stock logic)

UNS Trade family Seamless tube spec Welded tube spec Primary corrosion win
N02200 / N02201 Nickel 200/201 B161 / B163 B725 / B730 Caustic NaOH/KOH; 201 for >315°C
N04400 Monel 400 B163 / B165 B725 / B730 Seawater, brine, HF alkylation
N06600 Inconel 600 B163 / B167 B516 / B517 Oxidation, hot steam, chloride SCC resistance
N06625 Inconel 625 B163 / B444 B704 / B705 Hot seawater, sour service, high strength
N08800/810/811 Incoloy 800(H/HT) B163 / B407 B514 / B515 High-temp structural, reformer, HTA
N08825 Incoloy 825 B163 / B423 B704 / B705 H₂SO₄, H₃PO₄, chloride SCC, sour service
N10276 Hastelloy C-276 B622 B626 / B619 Mixed oxidising+reducing acids, FGD, wet Cl₂

B163 is the heat-exchanger/condenser workhorse; B161/B165/B167/B407/B423/B444/B622 are grade-specific seamless specs — never cross-label.

Stock Window (typical)

Parameter Range
OD 6-219mm (1/4"-8"); instrument capillary down to 0.2mm on request
Wall 0.5-12.7mm; SCH 5S-160
Length random 5-7m / fixed / U-bend / coiled
Condition annealed / solution-annealed / bright annealed / pickled
Form seamless tube, pipe, exchanger tube, U-bend, coiled tubing

Stock confirm within 4 business hours with OD×wall + UNS + medium/temp.

Seamless vs Welded — Don't Mix

  • Seamless: no longitudinal weld, preferred for high pressure, cyclic thermal load, sour service, exchanger bundles
  • Welded: B725/B730/B626 route, cost-efficient for larger OD/lower-risk duty — quoted only when PO invokes the welded spec
  • "Nickel alloy tube" without UNS + spec = incomplete order; we return it for completion, not substitution

QC Before Dispatch

  1. EN 10204 3.1 MTC — heat-specific chemistry + mechanicals, QA-independent signature
  2. PMI/OES per heat — UNS verified, not by colour or tag
  3. Hydrostatic test or eddy-current (B829 general requirements referenced)
  4. B163 flare test when exchanger spec invoked
  5. UT/dimensional/oval check; surface BA/AP/EP per PO
  6. Heat No. = bundle tag = MTC
  7. 3.2 (SGS/BV/TÜV/DNV) TPI PO-fronted, never back-built

Medium → Grade Quick Picker

  • NaOH/KOH, ≤315°C → N02200
  • NaOH/KOH, >315°C → N02201 (C≤0.02%)
  • Open seawater cooling → N06625 (hot/aerated) or Ti Gr2 (clean cold loop)
  • HF / hydrofluoric alkylation → N04400
  • Dilute/conc. H₂SO₄ + H₃PO₄ → N08825
  • Mixed acid + wet Cl₂ + FGD → N10276 (C-276)
  • High-temp oxidising gas → N06600/601 or N08810

Real Boundaries (no overclaim)

  • C-276 is versatile, not universal — confirm coupon data for unknown mixed streams
  • Monel 400 not for strong oxidisers (HNO₃ excursion)
  • 200/201 graphite rule stands: >315°C → 201 only
  • Nickel alloys weld only under qualified WPS/PQR (ASME IX F-No. grouping) — no stainless filler crossover
  • Storage: isolated from carbon steel, no sulphur/lead marker, clean slings

RFQ Template (copy-paste)

UNS / grade: N02200 / N02201 / N04400 / N06600 / N06625 / N08825 / N10276 ___
Spec: B161/B163/B165/B167/B407/B423/B444/B622 (+ welded if allowed) ___
OD × Wall: ___mm (or NPS × SCH ___)
Length: random / fixed ___mm / U-bend DWG / coil ___m
Condition: annealed / solution annealed / bright / pickled ___
Medium: ___ (concentration ___%, pH ___) + max temp ___°C
Test: hydro / eddy / flare(B163) / UT / IGC(ASTM G28/G48 if specified) ___
Cert: 3.1 / 3.2 TPI (SGS/BV/TÜV ___)
Qty: ___ m / ___ pcs
Incoterm: EXW Baoji / FOB Shanghai / CIF / DAP ___

FAQ — Corrosion Resistant Nickel Alloy Tube Stock

Q1: Which grade for caustic evaporator?
A: ≤315°C → N02200; >315°C → N02201 (C≤0.02%). Carbon value on MTC decides, not the tag.

Q2: Seawater — Monel or 625?
A: Clean cold loop often Ti Gr2; aerated/hot/chlorinated seawater → 625 (B444); HF-bearing brine → Monel 400.

Q3: Is B163 enough for exchanger tube?
A: Yes — B163 is the exchanger/condenser seamless spec; invoke flare test + avg/min wall basis explicitly.

Q4: Can welded tube replace seamless?
A: Only when PO invokes B725/B730/B626 and duty allows. Weld seam is a different risk path — not auto-substitutable.

Q5: How is grade verified, not assumed?
A: PMI/OES per heat + 3.1 MTC with actual chemistry. XRF alone misses carbon on low-C grades.

Q6: C-276 for everything?
A: Versatile, but over-spec = wasted budget. Use coupon/data for mixed streams; 825/625/Monel often correct and leaner.

Q7: U-bend / coiled tubing?
A: Yes — U-bend to bundle DWG, coiled instrument tubing continuous length on request.

Q8: 3.1 vs 3.2?
A: 3.1 = mill independent QA; 3.2 = +buyer-nominated TPI witness. Name TPI at PO, not after production.

Q9: HS code?
A: Nickel alloy tube common heading 7507 band — Broker confirms by destination/form.

Q10: Biggest procurement error?
A: PO says "nickel alloy tube" with no UNS, no medium, no temp. That's not a spec — it's a hope. Inspectors reject hopes.

Request a Quote

Email: sales@[yourdomain].com

Send OD×wall + UNS + medium/concentration/temp + qty. We recommend the grade from the stream, not the price list.


About: Baoji corrosion-resistant nickel alloy tube desk — N02200/201, N04400, N06600/625, N08800/825, N10276 seamless tube/pipe/exchanger tube. Grade matched to actual medium+temperature, ASTM B161/B163/B165/B167/B407/B423/B444/B622, PMI per heat, EN 10204 3.1, 3.2 TPI PO-fronted. No generic "nickel alloy" substitution, no welded-as-seamless, no broken heat chain. Heat No. = tag = MTC.

corrosion resistant nickel alloy tube stock N10276 N06625 N08825 seamless B163 MTC 3.1 Baoji / nickel alloy heat exchanger tube grade by medium caustic seawater acid

Get a Free Quote

Tell us your requirement — grade, size and quantity. We reply within 24 hours.

Captcha code

Prefer chat? WhatsApp +86 188 2967 9311 or email sales@sxqytd.com.