| Спецификация | We stock common OD and wall thickness sizes, support cut-length processing, offer clean packaging and complete export documents for chlor-alkali plant EPC contractors and end users. |
|---|---|
| Применимый стандарт | Manufactured from Nickel 200 UNS N02200 and tested under ASTM B161 norms, these tubes pass hydrostatic inspection and PMI identification, with traceable certification for alkali plant audit checks. |
| Состояние материала | Unlike stainless steel and titanium, pure nickel avoids caustic embrittlement and stress corrosion cracking in high-temperature lye environments, sustaining stable performance under continuous alkalin |
| Контроль и упаковка | We stock common OD and wall thickness sizes, support cut-length processing, offer clean packaging and complete export documents for chlor-alkali plant EPC contractors and end users. |
| Справочная цена | $50.00 – $60.00 |
Описание продукции: Pure Nickel 200 (UNS N02200) tube for caustic soda plant, ASTM B161 standard. Resists hot concentrated sodium hydroxide and caustic embrittlement, ideal for chlor-alkali electrolysis and evaporation l
Nickel 200 / N02200Nickel 201 / N02201ASTM B161 / B163EN 10204 3.1
The hotter and more concentrated the alkali, the more a plant needs pure nickel. That is the whole rule. Where austenitic stainless steels crack under hot concentrated caustic soda, pure nickel stays passive and stable.
Nickel 200 / 201 contains at least 99.0% nickel. Its self-healing oxide film handles sodium hydroxide and potassium hydroxide across the full concentration range at moderate temperatures — and unlike 304 or 316L, it does not fall apart in caustic stress-corrosion cracking.
Both grades share the same Ni≥99.0% chemistry. The split is carbon content, and carbon decides the service ceiling.
| Item | Nickel 200 (N02200) | Nickel 201 (N02201) |
|---|---|---|
| Carbon, max | 0.15% | 0.02% |
| Service ceiling | ≤315°C (600°F) | Up to ~650°C |
| Best fit | Standard caustic soda lines, ambient–moderate T | Hot-concentrated alkali, evaporators, high-T duty |
| Why the limit | Above 315°C, carbon precipitates as graphite at grain boundaries | Low carbon prevents graphite precipitation |
B161 and B163 are not interchangeable — one is general seamless pipe/tube, the other is condenser and heat-exchanger tubing. State the correct standard on the RFQ.
| Property | What it means in service |
|---|---|
| Ni ≥99.0% | Stable passive film in caustic, all concentrations, moderate temperatures |
| Caustic-SCC resistance | No alkali-induced stress-corrosion cracking like 300-series stainless |
| Thermal conductivity ~70 W/m·K | 3–5× austenitic stainless — evaporator tubes run efficiently |
| Density 8.89 g/cm³ | Heavier than titanium, lighter than copper-alloy alternatives in same duty |
| Non-contaminating | Suitable for food-grade and high-purity alkali handling |
| Property | Value |
|---|---|
| Tensile strength, min | ≥380 MPa (55 ksi) |
| Yield strength (0.2%), min | ≥105 MPa (15 ksi) |
| Elongation, min | ≥35–40% |
| Melting range | ~1435–1446°C |
| Parameter | Range |
|---|---|
| Outside diameter | 6–219 mm (1/2"–8"); fractional sizes on request |
| Wall / Schedule | SCH 5S, 10S, 40S, 80S, STD, XS, up to SCH 160 (confirmation required) |
| Length | Single / double random, or cut-to-length (commonly 3000–6000 mm) |
| Condition | Annealed, bright annealed, pickled; stress-relieved by agreement |
| Ends | Plain end / beveled end / threaded on request |
Live stock moves daily. Send OD × wall (or NPS × SCH) plus quantity for a same-day availability answer.
Welding uses ERNi-1 filler. Keep sulphur and lead away from the joint, and never drag a steel wire brush across nickel — cross-contamination ruins the surface.
Standard: ASTM B161 (pipe/tube) / B163 (exchanger tube) ___ Grade: N02200 (Nickel 200) / N02201 (Nickel 201) ___ OD: ___ mm (or NPS ___) Wall: ___ mm (or SCH ___) Length: random / fixed ___ mm Condition: annealed / bright annealed / pickled ___ Ends: plain / bevel / threaded ___ Service: NaOH/KOH concentration ___% Temp ___°C Test: hydrostatic / NDT / both ___ Cert: 3.1 / 3.2 (TPI ___) Quantity: ___ m / ___ pcs Incoterm: EXW Baoji / FOB Shanghai / DAP / DDP ___
Q1: Why pure nickel instead of 316L for caustic soda?
A: Because 316L is vulnerable to caustic stress-corrosion cracking as concentration and temperature rise. Pure nickel is not. That is the single reason chlor-alkali plants standardize on it.
Q2: 200 or 201 — how do I choose?
A: Service ≤315°C → Nickel 200. Service >315°C or any hot-concentrated alkali evaporator → Nickel 201. Carbon content is the deciding line.
Q3: Is graphite precipitation reversible?
A: No. Once carbon has precipitated at grain boundaries above the temperature limit, ductility does not come back. Prevention is the only option, which is why the grade decision is made before the PO.
Q4: Can pure nickel handle nitric acid?
A: Not as a default. Nitric is oxidizing acid — pure nickel belongs in reducing and alkaline duty. Send the exact medium and temperature for a proper alloy review.
Q5: What standard for heat-exchanger tubes?
A: ASTM B163 (SB-163). B161 covers general seamless pipe and tube, not condenser and exchanger tubing.
Q6: Is there stock, or is this all mill lead time?
A: Common sizes rotate in stock; heavy wall and unusual NPS are quoted to mill lead. Send dimensions and quantity for a fast availability check.
Q7: MTC with a small quantity?
A: EN 10204 3.1 with every lot. 3.2 is available when a TPI is named at the PO stage.
Q8: Does pure nickel contaminate high-purity caustic?
A: Nickel pick-up is negligible in caustic service, which is why it is used for high-purity alkali. Surface finish and cleaning state are agreed per application.
Q9: HS code for nickel tube?
A: Base 7506.20 for nickel tubes/pipes; the destination sub-heading must be confirmed with the buyer's broker.
Q10: What is the single biggest mistake buyers make?
A: Quoting 200 for a line that runs above 315°C to save cost. The right answer is 201 — and a supplier who quotes 200 without asking the temperature is not doing the job properly.
Email: sales@[yourdomain].com
Send OD × wall (or NPS × SCH) + grade + NaOH concentration + operating temperature + quantity. Stock answer within hours; dispatch window on heat confirmation.
About: Baoji nickel-tube desk — pure nickel tubes for caustic soda plants, ASTM B161 / SB-161 and ASTM B163 / SB-163, Nickel 200 (UNS N02200) for service to 315°C and Nickel 201 (UNS N02201) for high-temperature caustic evaporators. Annealed, cold-worked seamless, PMI verified, hydrostatic or NDT tested, EN 10204 3.1 with every lot and 3.2 available with PO-fronted TPI. No welded-passed-as-seamless, no grade mix, no 200 quoted above 315°C without flagging 201, no carbon confusion between 200 and 201. Heat number = tube tag = MTC.
Опишите ваши требования — марка, размер и количество. Ответим в течение 24 часов.
Предпочитаете чат? WhatsApp +86 188 2967 9311 или напишите на sales@sxqytd.com.
Контактное лицо: Wang Xiaoning
Телефон: +86-917-355-7966
Эл. почта: sales@sxqytd.com
WhatsApp: +86 188 2967 9311
Компания: Shaanxi Qianyi Tuoda Technology Co., Ltd
Адрес: Floor 4, Building 4, No. 188 Gaoxin Avenue, High-tech Zone, Baoji City, Shaanxi Province, China